Bonded Nd-Fe-B Compressed Magnet Material Properties

 

Material

Max. Energy Product

Residual Flux Density

Coercive Force

Intrinsic Coercive Force

Density

Recoil Permeability

Temp. Coefficient

Max. Operating Temperature

(BH) max

MGOe

Br

Gauss

Hc

Oe

Hci

Oe

D

g/cm3

m r

a Br

%/° C

Tw

° C

BNP-6

5-7

5,200-6,000

3800-4,500

8,000-10,000

5.3-5.8

1.15

-0.13

140

BNP-8

7-9

6,000-6,500

4,500-5,500

8,000-10,000

5.6-6.0

1.15

-0.13

140

BNP-10

9-10

6,500-7,000

4,500-5,800

8,000-10,000

5.8-6.1

1.22

-0.07~ - 0.105

120

BNP-12

10-12

7,000-7,600

5,300-6,000

8,000-10,000

6.0-6.2

1.22

-0.13

120

BNP-8H

6-9

5,500-6,200

5,000-6,000

12,000-16,000

5.6-6.0

1.15

-0.07~ - 0.13

120